Aka Mono plus 3 mic 250 ml


High Concentration Monocrystalline Diamond Suspension for metallographic specimen preparation.

 

  • 100% Mono crystalline diamonds

  • Median (50%) 2.84 µm. 

  • Tolerance 2.70 - 2.98 µm 

  • Upper limit (99%) 4.1 µm

  • Concentration 40 ct/l

Keep out of direct sunlight.